Steel-Wood Heat Insulation Fire Door
1. Door Case: 1.2 mm cold-rolled steel;
2. Door Leaf: Fire-retardant plywood or fire resistant paint-free plate;
3. Framework: Fire-retardant wood;
4. Thickness: 45mm;
5. Surface Finish: High temperature paint;
6. Selected wood: Fireproof pine;
7. Wood finish: Soaked for 4 hours in fire resistant fluid in a vacuum and high-pressure environment;
8. Process: Remove oil, remove rust, phosphate and passivation;
9. Internal Filler: Perlite--a new environmentally fire-retardant and adiabatic material;
10. Junction: Fireproof and sealed treatments, enhance the performance of fire prevention;
11. Type: Single, double, attached, with glass, and with bright windows;
12. Specification: 900× 2100, can customize as your requirement;
13. Fire Resistance Period: Grade A: 1.5h, Grade B: 1.0h, Grade C: 0.5h;
14. Hardware Accessories: Fire resistance period is above 1.5h.
Other supplier products
|
Steel Heat Insulation Fire Door |
1. Door Case: 1.2 mm galvanized steel;2. Door Leaf: 0.8 mm galvanized steel;3. Thickness: 50mm;4. Surface Finish: Spraying plastics and thermal tra... |
|
Steel-Wood Heat Insulation Fire Door |
1. Door Case: 1.2 mm cold-rolled steel;2. Door Leaf: Fire-retardant plywood or fire resistant paint-free plate;3. Framework: Fire-retardant wood;4.... |
|
Armoured Door |
1. Door Frame: 2.0 mm galvanized steel;2. Door Leaf: Macromolecular MDF sheet;3. Leaf Inside: 1.0 mm steel plate;4. Surface Finish: Shaped with inl... |
|
PVC Door / Paint Free Door |
1. Good fireproof performance,2. Simple structure,3. Corrosion resistance,4. Wind resistance,5. With anti-theft function at the same time6. Light w... |
|
solid wood door |
2. Thickness: 42mm;3. Wood Finish: Processed by special treatment, prevent the door leaf deformation and cracks;4. Surface Finish: Be coated wi... |
供应产品
Same products